Doing the whole job › Lesson 3 of 10 · 7 min read

Inspection, wear and condition grading

Once a movement is apart and roughly cleaned, you have a short window in which every defect is visible. Inspection is where you decide what the job really is. Do it under good light, with a loupe of at least 10×, a micrometer or vernier callipers, and a set of broaches or pin gauges. Do it before you repair anything, and write down what you find.

The measurements and limits in this lesson are working guides used by practitioners, not published standards. Clock tolerances depend on size, quality and purpose, so use them to make a sensible decision and apply judgement.

The wear check

PartWhat to look forHow to testAction
PivotsGrooves, pits, rust, flats, bends, tapered wear, burrs at the shoulder.Spin the arbor in a pivot holder or lathe; run a fingernail across the pivot; look under magnification. A groove you can catch with a nail is too deep to ignore.Light marks: polish with a pivot file and burnisher. Deep grooves or reduced diameter: repivot.
Pivot holesElongation in the direction of load, worn oil sinks, cracks, tapered wear.Insert the pivot and check for side-shake; look for a keyhole shape; broach gauge.Bush if clearance is excessive.
Teeth of wheelsHooked teeth, burrs, worn flanks, bent teeth, cracks, missing teeth.Look from the side at the tooth profile; compare teeth around the wheel.Straighten bent teeth; replace damaged teeth or fit a new wheel.
PinionsGrooves in the leaves, ridges at the root, rust, loose fit on the arbor.Look along the leaves for a worn pitch circle; check for a loose pinion.Polish light wear, replace badly worn pinions (turn the pinion leaves to a new pinion or replace the arbor).
Lantern pinionsWorn or loose trundles, bent trundles.Spin and check each trundle for wear and fit.Replace trundles or re-wire.
Escape wheelTooth tips thin or hooked, bent teeth, uneven spacing.Compare all teeth under magnification.Repair or replace.
Pallets and anchorGrooved faces, chipped corners, loose pallets, cracks.Look at faces in raking light.Polish lightly, re-face or replace; set pallets correctly.
Suspension springKinks, cracks, rust, broken ends.Inspect under magnification; check straightness and length.Replace if there is any doubt.
Crutch and forkWear on the fork, loose crutch on the arbor, bent rod.Check play at the pin and fork.Reduce the play; tighten.
Mainsprings and barrelsCracked or rusted spring, set spring, broken eyes, worn hook, scored barrel.Look for stains and deformities; check hooks.Replace tired springs; repair or replace barrel hooks.
Click workWorn click, click spring weak, ratchet teeth rounded.Look at the tips of the click and the ratchet teeth; test the click spring.Repair or replace.
Strike workWorn rack tail, worn snail, bent lifting piece, worn locking detent.Look at wear points and verify movement through the full range.Dress or repair; replace.
Motion workLoose cannon pinion (friction), worn teeth, bent pipe.Check friction fit by hand.Tighten the friction; replace the cannon.

Measuring side-shake and play at the pivots

Side-shake is the lateral play of a pivot in its hole. Measure it by measuring the pivot with a micrometer and the hole with a pin gauge or smoothing broach of known size.

Clearance = hole diameter − pivot diameter.

Worked example. A third-wheel pivot measures 1.00 mm. A hole gauge of 1.06 mm just enters the hole; 1.08 mm will not. The hole is about 1.06 mm. Clearance is 0.06 mm, or 6% of the pivot diameter. For a small clock a good guide for the working clearance is around 2 to 5% of the pivot diameter, so this is worn but acceptable on a non-critical wheel, and a candidate for bushing on the going train.

The error spreads through the train. A hole that is worn oval by 0.10 mm in the direction of the load changes the centre distance between the two wheels by up to 0.10 mm. For a wheel of module 0.5 mm the whole tooth depth is about 1.1 mm, so a 0.10 mm shift is about 9% of the depth. That is enough to make a depth too shallow or too deep, to cause tight spots and to waste power.

Clock classPivot diameterClearance guide (rule of thumb)Bush if
Carriage and platform escapement, small0.2 to 0.5 mm0.01 to 0.03 mmVisible shake at the plate when viewed under magnification, or an oval hole.
French and American mantel0.8 to 2 mm0.02 to 0.06 mmClearance over 0.10 mm, or an oval hole.
Longcase and bracket1.5 to 4 mm0.04 to 0.10 mmClearance over 0.15 mm, or an oval hole.

These figures are a good rule of thumb and a guide, not a rule. The underlying requirement is that every part moves freely with minimal shake. Going-train holes (centre to escape) matter more than strike-train holes, because they set the depths that determine the rate and the amplitude.

Measuring end-shake

End-shake is the axial play of an arbor between the plates. It must exist so the arbor can turn without pressing on the plate, but too much allows wheels to move out of mesh and pinions to ride on the edges of the teeth.

  1. With the movement assembled on the plates (pillars fitted, plates pinned), lift each arbor in turn with a fine tool and note the movement.
  2. Measure it with a feeler gauge, a depth gauge, or a dial indicator, or compare it with a known thickness.
  3. Record the result.
MovementTypical end-shake (a guide)
Platform or watch-sized parts0.02 to 0.05 mm
French carriage and small mantel0.10 to 0.20 mm
American and German mantel0.15 to 0.30 mm
English bracket and longcase0.20 to 0.50 mm

These figures are a good rule of thumb and a guide, not a rule. The underlying requirement is that every part moves freely with minimal shake. Too little end-shake makes the arbor bind; too much makes the strike and going trains unreliable. If end-shake is wrong, it can be corrected by adjusting the shoulder, the bush or the pivot length.

Depth, alignment and plates

Condition grading

Grade each part, then the whole movement. Grading makes the repair plan easier, and it gives you a record to compare with later. The scale below is a practical shop scale, not an industry standard.

GradeMeaningTypical action
AAs new or lightly worn; no repair needed.Clean and oil.
BLight wear; will function well with cleaning and polishing.Polish pivots and surfaces.
CModerate wear; repair needed to last.Bush holes, repair pivots, repair teeth.
DSevere wear or damage; replacement or major repair.New wheel, pinion or arbor; new barrel; escapement repair.

Record a row for each train and for the main groups. A simple table works.

ItemPartGradeNotes
Going trainPivots
Going trainHoles
Going trainWheels and pinions
EscapementPallets and escape wheel
Strike trainPivots and holes
Strike trainWheels and pinions
Strike workRack, snail, levers
SpringsCondition
Plates and pillarsCondition
Case, dial, handsCondition

Count the C and D grades. A movement with many Cs is a full restoration, not a service. Tell the owner and update the plan.

Look for the cause, not just the symptom. Wear usually has a reason: a bent pivot, a poorly set depth, a rusty spring, too little oil, too much oil, grit. If you repair the wear and leave the cause, the repair will not last.
Check your work. Every wheel must turn freely by hand in the plates; the pivots must have a visible shine, with no pits; and the holes must have crisp oil sinks.
Sources

Spring failure modes (cracking at the eye, set, rust) are described from workshop experience; I found no authoritative source I could read for them.

The clearances, end-shake figures and grading scale above are workshop guides, not rules and not figures from a published standard.

Get new lessons by email

Free, practical clock repair lessons for beginners. No spam, unsubscribe any time.